What to Know About Liquid Coating

August 1, 2022 by SWhite

When you need coatings for computer, lighting, scientific, medical, building, aerospace, and military equipment, you might not know where to start. Should you start with powder coating or liquid coating? With the demand from the coating industry rising at an average rate of 3% per year from 2016 to 2021, it’s clear that coating services are on the rise. Keep reading here to learn what you need to know about liquid coating before you get started.

There’s a Great Variety of Options

With so many paint options to choose from at Professional Finishing, it’s easy to get the exact combination of coatings that you’ve imagined. We can recommend the right preparation, primer, and paint option to meet your end user’s expectations. Paint is also the right option to go with when you need to cover certain substrates, including plastic and wood. Here are some of the finishes we offer:

  • Polyurethane
  • Epoxy
  • Water Borne
  • Dry Film Lubricant

It’s Economical

The economical benefits of liquid coating cannot be overlooked. Because liquid can be manufactured in small batches, it’s less expensive than comparable options. It’s also a cheap color-matching process than powder coating. Liquid coatings are also thinner than other options, so less material is needed to cover vast areas. This is a great money-saving tactic for all grades of coating. This is true for all sizes of projects!

There’s Little Risk Involved

With liquid coating, there will be a greater margin for error than there is with other options. This is due to the low occurrence of film builds, which can result in a large number of rejected products. With the robotic systems at Professional Finishing, there’s even less chance of errors occurring during painting. We have both conveyorized robotic booths and robotic spray booths, both of which can handle your next project. With low cost, low error rate, and a variety of options, you can’t go wrong when choosing to use a liquid coating process.

With so many choices for coating your materials and products, it’s good to start out with some research. When you want to get started with a new liquid or powder coating company, take a look at our services online. We can help you choose the right method for your next project.

Filed Under: Uncategorized

Footer

Now in three locations:

Richmond, CA

Harlingen, TX

Hayward, CA

Contact

Professional Finishing
Headquarters
770 Market Avenue
Richmond, CA 94801
Get Directions
510.233.7629
Let's Work Together

Menu

  • Home
  • About Us
    • Press
  • Industries
    • Appliances
    • Architecture
    • Electronics
    • Furniture
    • Lighting
    • Medical
    • Retail
  • Industrial Powder Coating Services
    • Liquid Coating
    • Powder Coating
    • Precision Masking
    • Sandblasting
  • Projects
  • Contact Us
  • Quote Genius Pro

Terms and Conditions

Blog

Capabilities

© 2026 · Professional Finishing